Add to Cart
the saturation magnetization, and of embrittling the alloy when the silicon additions exceed about 2 wt.%. The embrittling effects of silicon make it difficult to produce silicon steels with more than about 3 wt.% silicon. The silicon steels are produced in two forms, highly textured grain-oriented alloys and alloys in which the grains are not oriented. Grain orientation is carried out to align the magnetic easy axis.
Type | Nominal thickness (mm) | Tensile strength L (N/mm2) | Yield strength L (N/mm2) | Elongation L (%) | Hardness HV1 | Number of bends | Lamination factor (%) |
Common series | 0.27 | 335 | 305 | 12 | 190 | 25 | 97.5 |
0.3 | 345 | 310 | 12 | 190 | 20 | 98 | |
High induction series | 0.23 | 351 | 316 | 10 | 197 | 22 | 96.5 |
0.27 | 350 | 325 | 12 | 195 | 20 | 97.5 | |
0.3 | 350 | 310 | 11 | 195 | 17 | 98 | |
Domain refined high induction series | 0.23 | 353 | 326 | 12 | 195 | 19 | 96.5 |
0.27 | 355 | 330 | 10 | 200 | 18 | 97.5 |